This chapter discusses the role of inverse analysis in providing input data for finite element simulations of metal forming processes. It describes the basic procedures for determining flow stress and friction by inverse analysis and for comparing experimental measurements with corresponding computed data. It also includes an example in which flow stress and friction were measured in compressed aluminum rings and the results used to verify the accuracy of predicted values.