Chapter 15: Beryllium Binary Phase Diagrams
By
Loren A. Jacobson
Loren A. Jacobson
Los Alamos National Laboratory
Retired
Search for other works by this author on:
-
Published:2009
Abstract
This chapter is a compilation of beryllium phase diagrams, representing more than 25 binary alloy systems from beryllium-aluminum to beryllium-zirconium. Each diagram is presented along with a summary and source reference.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Loren A. Jacobson, Beryllium Binary Phase Diagrams, Beryllium Chemistry and Processing, By Kenneth A. Walsh;Edited By Edgar E. Vidal, Alfred Goldberg, Edward N.C. Dalder, David L. Olson, Brajendra Mishra, ASM International, 2009, p 179–197, https://doi.org/10.31399/asm.tb.bcp.t52230179
Download citation file:
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.
Related Topics
Related Book Content
Introduction to Phase Diagrams
Phase Diagrams Understanding the Basics
Intermediate Phases
Alloy Phase Diagrams