Beryllium is the 44th most abundant element on Earth, with an estimated concentration of six parts per million in the Earth’s crust. It is found in various forms in more than 100 minerals, two of which, beryl and bertrandite, account for most of the beryllium produced throughout the world. This chapter describes where and how beryllium is obtained and provides facts, figures, and insights on global supply and demand.