Abstract

Resistance welding is a group of processes in which the heat for welding is generated by the resistance to the flow of an electrical current through the parts being joined. This chapter discusses the processes, advantages, and limitations of specific resistance welding processes, namely resistance spot welding, resistance seam welding, projection welding, flash welding, and upset welding.