Case 37: Failure of an Aileron Control Cable in an Aircraft
-
Published:2005
Abstract
This chapter discusses the failure of an aileron control cable in an aircraft and explains how investigators determined the cause. Based on their observations and the results of SEM fractography, investigators concluded that the cable had been damaged by a shearing tool, leading to its failure.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Failure of an Aileron Control Cable in an Aircraft, Failure Analysis of Engineering Structures: Methodology and Case Histories, By V. Ramachandran, A.C. Raghuram, R.V. Krishnan, S.K. Bhaumik, ASM International, 2005, p 152–153, https://doi.org/10.31399/asm.tb.faesmch.t51270152
Download citation file:
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.
Related Book Content
Fractographic and Metallographic Study of Spalling Failure of Steel Straightener Rolls
Handbook of Case Histories in Failure Analysis
Photography of Fractured Parts and Fracture Surfaces
Fractography
Use of Fractography for Failure Analysis
Metals Handbook Desk Edition, 2nd Ed. (2nd Edition)
Scanning Electron Microscopy
Materials Characterization (2019 Edition)
Study on Failure Analyses and Material Characterizations of a Damaged Booster Pump
Handbook of Case Histories in Failure Analysis
Failure Analysis of Open End Wrenches Containing Forging Defects
Handbook of Case Histories in Failure Analysis
Electrical Fluting Failure of a Tri-Lobe Roller Bearing
Handbook of Case Histories in Failure Analysis
Failure Analysis of NiTi Wires Used in Medical Applications
Handbook of Case Histories in Failure Analysis
Stress Corrosion Cracking of Tough Pitch Copper in a Bolting Application
Handbook of Case Histories in Failure Analysis
Failure Localization with Active and Passive Voltage Contrast in FIB and SEM
Microelectronics Failure Analysis: Desk Reference (Seventh Edition)