Chapter 9: Liquid Penetrant, Magnetic Particle, and Eddy-Current Inspection
-
Published:2013
Abstract
Liquid penetrant, magnetic particle, and eddy current inspection are used to detect surface flaws. This chapter is a detailed account of the physical principles, process description, equipment requirements, selection criteria, advantages, limitations, and applications of these surface flaw detection techniques.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Liquid Penetrant, Magnetic Particle, and Eddy-Current Inspection, Inspection of Metals: Understanding the Basics, Edited By F.C. Campbell, ASM International, 2013, p 183–232, https://doi.org/10.31399/asm.tb.imub.t53720183
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.