Inspection of Metals: Understanding the Basics
Chapter 6: Tensile Testing
-
Published:2013
Abstract
This chapter is a detailed account of the tensile testing procedure used for evaluating metals and alloys. The discussion covers the stress-strain behavior of metals determined by tensile testing, properties determined from testing, test machines for measuring mechanical properties, and general procedures of tensile testing. Three distinct aspects of standard test methods for tension testing of metallic materials are discussed: test piece preparation, geometry, and material condition; test setup and equipment; and test procedure.
Sign in
ASM members
Member Sign InTensile Testing, Inspection of Metals: Understanding the Basics, Edited By F.C. Campbell, ASM International, 2013, p 117–138, https://doi.org/10.31399/asm.tb.imub.t53720117
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.