Abstract

This article explains how alloying elements affect the properties and behaviors of electrical contacts. It describes the composition, strength, hardness, and conductivity of a wide range of contact alloys and composites based on silver, copper, gold, platinum, palladium, tungsten, and molybdenum, and related oxides and carbides.