Alloying: Understanding the Basics
Stainless Steels and Heat-Resistant Alloys
-
Published:2001
Abstract
This article covers the metallurgy and properties of stainless steels. It provides composition information on all types of ferritic, austenitic, martensitic, duplex, and precipitation-hardening stainless steels, including proprietary and nonstandard grades, along with corresponding property and performance data. It also discusses the effect of various alloying elements on pitting, crevice corrosion, sensitization, stress-corrosion cracking, and oxidation resistance.
Abstract
This article discusses the composition, structure, and properties of iron-nickel-, nickel-, and cobalt-base superalloys and the effect of major alloying and trace elements. It describes the primary and secondary roles of each alloying element, the amounts typically used, and the corresponding effect on properties and microstructure. It also covers mechanical alloying and weldability and includes nominal composition data on many wrought and cast superalloys.
Sign in
ASM members
Member Sign InStainless Steels and Heat-Resistant Alloys, Alloying: Understanding the Basics, Edited By J.R. Davis, ASM International, 2001
Download citation file: