Book Chapter
Chapter 2: Engineering Component Configuration
-
Published:2018
Abstract
This chapter is a brief account of various factors pertinent to the development of an engineering component. The discussion covers the disciplines and interactions of design development, engineering of component design, validation of design and process analysis, and matrix of design and manufacturing elements.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Engineering Component Configuration, Aluminum Castings Engineering Guide, By Jagan Nath, ASM International, 2018, p 9–19, https://doi.org/10.31399/asm.tb.aceg.t68410009
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.