Abstract

This appendix contains a table listing cross-references of standard SAE carbon and low-alloy steels to selected chemically similar steels.

You do not currently have access to this chapter.
Don't already have an account? Register

2008. "AISI to Non-AISI Steel Cross Reference", Failure Analysis of Heat Treated Steel Components, Lauralice de C.F. Canale, Rafael A. Mesquita, George E. Totten