Abstract
This chapter discusses some of the metallurgical factors that affect corrosion of weldments and describes a few considerations for selected nonferrous alloy systems: aluminum, titanium, tantalum, and nickel.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Corrosion of Nonferrous Alloy Weldments, Corrosion in the Petrochemical Industry, 2nd ed., Edited By Victoria Burt, ASM International, 2015, p 112–116, https://doi.org/10.31399/asm.tb.cpi2.t55030112
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.