Abstract
The Nuclear Waste Management Organization (NWMO) investigates approaches for managing Canada's used nuclear fuel. As part of a larger program investigating concepts of copper coatings, NWMO has begun exploring copper cold spray in collaboration with the National Research Council. Within the coating program, a large variety of copper coating sizes have been investigated, from small corrosion coupons to full-scale used-fuel containers/canisters (UFCs). This chapter demonstrates the successful application of copper coating technology to full-scale geometric representative Mark II UFC mock-up configurations through activities involving powder selection, general coating development, UFC coating optimization, and prototyping.
Sign in
ASM members
Member Sign InP. Vo, D. Poirier, J.-G. Legoux, E. Irissou, P.G. Keech, Application of Copper Coatings onto Used-Fuel Canisters for the Canadian Nuclear Industry, High Pressure Cold Spray: Principles and Applications, Edited By Charles M. Kay, J. Karthikeyan, ASM International, 2016, p 253–276, https://doi.org/10.31399/asm.tb.hpcspa.t54460253
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.