This chapter discusses the application of high-pressure cold spray to the automotive industry field, with special attention to three applications: additive manufacturing, fabrication methods, and protective coatings. Various studies on the automotive application of cold spray are reviewed. The background and purpose of each application are presented and practical cases are discussed.

You do not currently have access to this chapter.
Don't already have an account? Register

C. Lee, J. Kim, Cold Spray Applications in the Automotive Industry, High Pressure Cold Spray: Principles and Applications, Edited By Charles M. Kay, J. Karthikeyan, ASM International, 2016, p 209–226, https://doi.org/10.31399/asm.tb.hpcspa.t54460209