High Pressure Cold Spray: Principles and Applications
Chapter 4: Cold Spray Equipment
-
Published:2016
Abstract
This chapter provides an overview of the state of the art in high-pressure cold spray equipment, including both spray systems and gas supply systems. The chapter describes the commercial cold spray systems developed by companies such as Cold Gas Technology (CGT) GmbH, Plasma Giken Company Ltd, Impact Innovations GmbH, and ASB Industries. Typical helium and nitrogen gas systems used in high-pressure cold spray processing are reviewed.