Characterization and Failure Analysis of Plastics
Edited by
ASM International
ISBN electronic:
978-1-62708-281-5
Publication date:
2003
Abstract
The susceptibility of plastics to environmental failure, when exposed to organic chemicals, limits their use in many applications. Environmental factors can be classified into two categories: chemical and physical effects. This article discusses the effects of these environmental factors on the mechanical properties of plastics.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Organic Chemical Related Failure, Characterization and Failure Analysis of Plastics, Edited By Steven Lampman, ASM International, 2003, p 323–328, https://doi.org/10.31399/asm.tb.cfap.t69780323
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.
Related Topics
Related Book Content
Introduction to Engineering Plastics
Engineered Materials Handbook Desk Edition
Superalloys
Metals Handbook Desk Edition, 2nd Ed. (2nd Edition)
Corrosion Resistance of Magnesium and Magnesium Alloys
Metals Handbook Desk Edition, 2nd Ed. (2nd Edition)
Electroless Nickel Plating
Surface Engineering
Wear Failures of Plastics
Failure Analysis and Prevention
Mechanical Testing and Properties of Plastics: An Introduction
Characterization and Failure Analysis of Plastics
Corrosion by Alkalis
Corrosion: Environments and Industries
Corrosion by Phosphoric Acid
Corrosion: Environments and Industries
Corrosion of Metal Artifacts and Works of Art in Museum and Collection Environments
Corrosion: Environments and Industries
Investment Casting
Casting