This chapter focuses on key requirements for obtaining third-generation advanced high-strength steels (AHSS). The discussion covers the microstructure design for AHSS, novel AHSS processing routes, the development of nanostructured AHSS, and the development of third-generation AHSS by the Integrated Computational Materials Engineering approach.