Advanced-High Strength Steels: Science, Technology, and Applications
Chapter 15: Innovative Forming Technologies
-
Published:2013
Abstract
The increased use of advanced high-strength steels to achieve weight reduction in automobiles has led to the development of innovative tool designs and manufacturing processes. Among these technologies and processes are: real-time process control, active drawbeads, active binders, flexible binders, and flexible rolling. This chapter presents the implementation, advantages, disadvantages, and applications of these processes and technologies.