This chapter provides information on ultra-light steel family research programs conducted by the global steel industry under the umbrella of WorldAutoSteel. It discusses the collaboration efforts between U.S government, industry, and academia on advanced high-strength steels (AHSS) technology. Some of the projects on AHSS research and development are also reviewed.