This appendix contains tables listing the composition of austenitic, ferrite, martensitic, precipitation-hardenable, and duplex stainless steels and of Alloy Casting Institute heat- and corrosion-resisting casting alloys.

Abstract

This appendix contains tables listing the physical and mechanical properties of stainless steel engineering alloys. The physical properties covered are density, modulus of elasticity, coefficient of thermal expansion, thermal conductivity, specific heat, and electrical resistivity. The mechanical properties listed include yield strength, tensile strength, elongation and hardness.

Abstract

This appendix provides a brief introduction to Thermo-Calc, explains what it is, and lists its uses. Instructions for accessing a demonstration version of the software are also provided.

You do not currently have access to this chapter.
Don't already have an account? Register

Appendices, Stainless Steels for Design Engineers, By Michael F. McGuire, ASM International, 2008

Download citation file:


Close
Close Modal

or Create an Account

Close Modal
Close Modal