Chapter 24: Pulp-and-Paper Industry Applications
-
Published:2008
Abstract
This chapter is a brief account of the applications of stainless steel in processes pertinent to the pulp-and-paper industry.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Pulp-and-Paper Industry Applications, Stainless Steels for Design Engineers, By Michael F. McGuire, ASM International, 2008, p 265–267, https://doi.org/10.31399/asm.tb.ssde.t52310265
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.