Abstract

This chapter discusses different thermal processes applicable to the various alloy groups of stainless steels, namely austenitic, ferritic, martensitic, precipitation hardening, and duplex stainless steels. The processes discussed include soaking, annealing, stress relieving, austenitizing, tempering, aging, and conditioning.