Chapter 10: Precipitation-Hardening Stainless Steels
-
Published:2008
Abstract
This chapter discusses the composition, alloying characteristics, mechanical properties, corrosion resistance, advantages, limitations, and applications of martensitic, semiaustenitic, and austenitic precipitation-hardenable stainless steels.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Precipitation-Hardening Stainless Steels, Stainless Steels for Design Engineers, By Michael F. McGuire, ASM International, 2008, p 137–146, https://doi.org/10.31399/asm.tb.ssde.t52310137
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.