Abstract

This chapter explores the behavior of stainless steel in media that promote corrosion. The forms of corrosion covered are uniform corrosion, atmospheric corrosion, localized corrosion, pitting corrosion, crevice corrosion, and grain boundary corrosion. The chapter discusses the influence of material and environmental variables on stress-corrosion cracking (SCC) and the mechanisms proposed for SCC in stainless steel, comparing the mechanism of SCC with hydrogen embrittlement. In addition, it provides information on biocorrosion and microbiologically induced corrosion in ambient aqueous environments.