This appendix includes a temperature conversion table, a table containing equivalent hardness numbers, and a unit conversion table.

You do not currently have access to this chapter.
Don't already have an account? Register

Conversion Tables, Light Microscopy of Carbon Steels, By Leonard E. Samuels, ASM International, 1999, p 459–464, https://doi.org/10.31399/asm.tb.lmcs.t66560459