Abstract

This appendix is a compilation of tables helpful to metallographers in characterizing irons and steels. The tables include AISI/SAE designations and specific composition ranges for various steels and irons, listings of companies that sell metallographic equipment and supplies, and compositions and usage guidance for etchants, chemical polishing solutions, and coatings.

This content is PDF only. Please click on the PDF icon to access.