This chapter describes surface modification processes that go beyond conventional heat treatments, including plasma nitriding, plasma carburizing, low-pressure carburizing, ion implantation, physical and chemical vapor deposition, salt bath coating, and transformation hardening via high-energy laser and electron beams. The chapter compares methods and includes several example applications.

You do not currently have access to this chapter.
Don't already have an account? Register

Surface Modification, Steels: Processing, Structure, and Performance, 2nd ed., By George Krauss, ASM International, 2015, p 551–577, https://doi.org/10.31399/asm.tb.spsp2.t54410551