This chapter discusses the stress-strain response of ferritic microstructures and its influence on tensile deformation, strain hardening, and ductile fracture of carbon steels. It describes the ductile-to-brittle transition that occurs in bcc ferrite, the effects of aging and grain size on strength and toughness, continuous and discontinuous yielding behaviors, and dispersion and solid-solution strengthening processes.

You do not currently have access to this chapter.
Don't already have an account? Register

Deformation, Strengthening, and Fracture of Ferritic Microstructures, Steels: Processing, Structure, and Performance, 2nd ed., By George Krauss, ASM International, 2015, p 213–232, https://doi.org/10.31399/asm.tb.spsp2.t54410213