Skip Nav Destination
ASM Handbook
Materials Characterization (2019 Edition)
ASM International
Volume
10
ISBN electronic:
978-1-62708-213-6
Publication date:
2019
Book Chapter
Semiconductor Characterization
-
Published:2019
Abstract
This article introduces various techniques commonly used in the characterization of semiconductors, namely single-crystal, polycrystalline, amorphous, oxide, organic, and low-dimensional semiconductors and semiconductor devices. The discussion covers material classification, fabrication methods, sample preparation, bulk/elemental characterization methods, microstructural characterization methods, surface characterization methods, and electronic characterization methods.
You do not currently have access to this chapter.
Citation
David T. Schoen, Meredith S. Nevius, Sumit Chaudhary, Semiconductor Characterization, Materials Characterization, Vol 10, 2019 ed., ASM Handbook, ASM International, 2019, p 11–28, https://doi.org/10.31399/asm.hb.v10.a0006670
Download citation file: