ASM Handbook
Materials Characterization (2019 Edition)
ASM International
Volume
10
ISBN electronic:
978-1-62708-213-6
Publication date:
2019
Search within book:
Abstract
This article discusses several purposes and types of materials characterization techniques. Some of the factors to be considered when selecting appropriate characterization methods are described. The article also presents the scope and organization of this volume.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Introduction to Materials Characterization, Materials Characterization, Vol 10, 2019 ed., ASM Handbook, ASM International, 2019, p 3–4, https://doi.org/10.31399/asm.hb.v10.a0006669
Download citation file:
Understanding the Basics Collection
8-Volume Digital Library Exclusive
The Understanding the Basics Collection provides comprehensive coverage of critical topics in metallurgy. These introductory guides present critical information on key topics related to materials processing, performance, and evaluation.
Related Book Content
Introduction and Overview of Materials Characterization
Metals Handbook Desk Edition (2nd Edition)
High-Temperature Combustion
Materials Characterization
X-Ray Diffraction Residual Stress Techniques
Materials Characterization
Microstructure and Domain Imaging of Magnetic Materials
Metallography and Microstructures