Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Article Type
Volume Subject Area
Date
Availability
1-2 of 2
Wen-Fei Hsieh
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Proceedings Papers
ISTFA2023, ISTFA 2023: Conference Proceedings from the 49th International Symposium for Testing and Failure Analysis, 209-213, November 12–16, 2023,
Abstract
View Papertitled, The Sulfide Contamination Management in Circuit Probing FAB Clean Room Environment
View
PDF
for content titled, The Sulfide Contamination Management in Circuit Probing FAB Clean Room Environment
Sulfur corrodes silver metal in a continuous reaction. This corrosion is also found in semiconductor industry processes for the application of silver into Backside Grinding & Backside Metal (BGBM). In this paper two experiments were conducted for the sulfide corrosion behavior in a Circuit Probing (CP) clean room environment. They were Mixed Flowing Gas (MFG) and clean room environment exposure test. The MFG test of this research was conducted in a testing chamber with temperature, relative humidity, and concentration of H2S were carefully controlled and monitored. The MFG test conditions included the test temperature of 25°C, relative humidity of 75 %, and H 2 S gas concentration of 10 ppb. And the MFG tests lasted for over 72 hours. The X-ray photoelectron spectroscopy (XPS) was used to analyze the elements composition and Ag 2 S film thickness of the MFG test samples. The second test of this research was the direct exposure experiment. The silicon samples deposited with appropriate silver layer thickness were exposed in CP fab clean room environment with H 2 S concentration well monitored. The XPS analysis results of the corresponding exposure test samples indicated that the Ag 2 S contamination would continue to develop and wouldn't saturate. This would be indicative for the management of Ag 2 S contamination control. The results of MFG and Exposure test were help for Ardentec to setup Ag 2 S corrosion methodology. All the managements were applied into daily operation of the BGBM semiconductor products.
Proceedings Papers
ISTFA2009, ISTFA 2009: Conference Proceedings from the 35th International Symposium for Testing and Failure Analysis, 214-216, November 15–19, 2009,
Abstract
View Papertitled, The Novel TEM Sample Preparation Approach for Targeted via with Barrier/Cu Seed Layer Inspection
View
PDF
for content titled, The Novel TEM Sample Preparation Approach for Targeted via with Barrier/Cu Seed Layer Inspection
In this study, an FIB-based cross section TEM sample preparation procedure for targeted via with barrier/Cu seed layer is introduced. The dual beam FIB with electron beam for target location and Ga ion beam for sample milling is the main tool for the targeted via with barrier/Cu seed layer inspection. With the help of the FIB operation and epoxy layer protection, ta cross section TEM sample at a targeted via with barrier/Cu seed layer could be made. Subsequent TEM inspection is used to verify the quality of the structure. This approach was used in the Cu process integration performance monitor. All these TEM results are very helpful in process development and yield improvement.