Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Article Type
Volume Subject Area
Date
Availability
1-1 of 1
U. Somboon
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Proceedings Papers
Corrosion Fatigue Properties of Al 2 O 3 Plasma-Sprayed SUS316L Stainless Steel in a Physiological Saline Solution
Available to Purchase
ITSC 2001, Thermal Spray 2001: Proceedings from the International Thermal Spray Conference, 1171-1178, May 28–30, 2001,
Abstract
View Papertitled, Corrosion Fatigue Properties of Al 2 O 3 Plasma-Sprayed SUS316L Stainless Steel in a Physiological Saline Solution
View
PDF
for content titled, Corrosion Fatigue Properties of Al 2 O 3 Plasma-Sprayed SUS316L Stainless Steel in a Physiological Saline Solution
The SUS316L stainless steel rod specimen coated with plasma-sprayed Al 2 O 3 deposits has been fatigued in a physiological saline solution (0.9 % NaCl solution) to evaluate the potential of its application to prosthetic implant materials. Push-pull loading fatigue tests were conducted at the stress ratio of R = -1, and at the frequency of 2 Hz. Pure titanium powder was selected for undercoat. Fatigue damage was examined on longitudinal section of the specimen and fracture surface by optical and electron microscopy from the microstructural viewpoints. The plasma spraying of Al 2 O 3 powder has significantly improved fatigue properties of the substrate metal in the longer range of fatigue lives, compared with the results of the non-coated steel specimen. It was found from electrochemical experiments that titanium for undercoat metal has acted as sacrificial anode to protect the substrate metal from corrosive attack and under lower stress amplitudes the plasma sprayed Al 2 O 3 coating kept the solution out at an early stage of fatigue lives. Fatigue cracks preferentially originated from flaws, which had been caused on the substrate metal surface through grit blasting, and extended into the bulk of substrate metal. Fatigue cracks appear not to develop into plasma-sprayed deposits while the deposits could accommodate themselves to the crack opening displacement at the surface of substrate metal. It was understood that the plasma sprayed coating has enhanced fatigue properties in the solution both by keeping the solution out during the early stage of fatigue lives and by electrochemical effects of the undercoat metal when the topcoat was cracked in macroscopic scale.