Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Article Type
Date
Availability
1-1 of 1
Tony Studer
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Proceedings Papers
AM-EPRI2024, Advances in Materials, Manufacturing, and Repair for Power Plants: Proceedings from the Tenth International Conference, 1075-1086, February 25–28, 2025,
Abstract
View Papertitled, Cracking of Grade 91 Steel Welds in Longer-Term Service - Case Studies
View
PDF
for content titled, Cracking of Grade 91 Steel Welds in Longer-Term Service - Case Studies
This paper presents three recent example cases of cracking in Grade 91 steel welds in longer-term service in high temperature steam piping systems: two girth butt welds and one trunnion attachment weld. All the cases were in larger diameter hot reheat piping, with the service exposure of the welds ranging from approximately 85,000 to 150,000 hours. Cracking in all cases occurred by creep damage (cavitation and microcracking) in the partially transformed heat-affected zone (PTZ, aka Type IV zone) in the base metal adjacent to the welds. The location and morphology of the cracking are presented for each case along with operating conditions and potential contributors to the cracking, such as system loading, base metal chemical composition, and base metal microstructure.