Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Subjects
Article Type
Volume Subject Area
Date
Availability
1-1 of 1
Tom Ignatowski
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Proceedings Papers
HT2017, Heat Treat 2017: Proceedings from the 29th Heat Treating Society Conference and Exposition, 524-533, October 24–26, 2017,
Abstract
View Paper
PDF
High frequency welding is a thermo-mechanical process that relies on precise heat input as well as mechanical control as strip edges are heated and forged together to result in a seam weld. Heat input can be defined as a way of characterizing the temperature distribution at the strip edges prior to forging them together. Heat input is affected by several process variables ranging from raw material properties to welder settings and weld area setup. These are summarized in this paper, with special attention on the effects of welder frequency, welder power, line speed, and steel alloy composition on heat input and the resulting weld quality. Frequencies in the range of 100 – 800 kHz are considered. Data from tube mills (including general data and controlled on-the-mill experiments) and laboratory evaluations are included in this paper.