Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Article Type
Volume Subject Area
Date
Availability
1-1 of 1
T. Reinhardt
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Proceedings Papers
ITSC1999, Thermal Spray 1999: Proceedings from the United Thermal Spray Conference, 128-133, March 17–19, 1999,
Abstract
View Papertitled, Development and Application of TiC-Ni-Based Plasma Sprayed Coatings
View
PDF
for content titled, Development and Application of TiC-Ni-Based Plasma Sprayed Coatings
TiC-based coatings sprayed by different processes, such as detonation gun spraying, high velocity oxy-fuel spraying, atmospheric plasma spraying (APS), and vacuum plasma spraying, using agglomerated and sintered powders have been actively developed over the years. This development is based on the high technical and engineering potential of the hard phase TiC. This paper describes the results of basic studies of the APS for various alloying steps in the production of TiC base coatings from agglomerated and sintered powders as well as the results of the application of APS coatings on piston rings. Paper includes a German-language abstract.