Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Article Type
Volume Subject Area
Date
Availability
1-8 of 8
T. Li
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Proceedings Papers
ITSC2014, Thermal Spray 2014: Proceedings from the International Thermal Spray Conference, 733-738, May 21–23, 2014,
Abstract
View Paper
PDF
In cold spraying, several theories have been presented to explain the bonding between the substrate and coatings. In this work, finite element simulations were performed to obtain the minimal bonding strength to overcome rebounding at different initial velocities. The correlation with critical deposition velocity is also discussed.
Proceedings Papers
ITSC2014, Thermal Spray 2014: Proceedings from the International Thermal Spray Conference, 842-844, May 21–23, 2014,
Abstract
View Paper
PDF
Aluminum-titanium powder mixtures were deposited on γ-TiAl alloy substrates by cold spraying then heat treated for 5 h at 600, 650, and 700 °C. SEM and XRD examination showed that the treatment caused Al to diffuse into the substrate where it reacted with Ti, resulting in changes in microstructure. The diffusion of Al left pores in the fringes of the TiAl 3 phase, increasing the porosity of the coatings. A surplus of Al remained in the coatings after heat treatment at 600-650 °C, but at 700 °C, all Al was consumed, contributing to the formation of a continuous TiAl 3 layer.
Proceedings Papers
ITSC2014, Thermal Spray 2014: Proceedings from the International Thermal Spray Conference, 845-848, May 21–23, 2014,
Abstract
View Paper
PDF
This study investigates the microstructure, thermal conductivity, hardness, and strength of Cu-Cr-Zr coatings produced by cold gas spraying. The elements in the powders were found to have a significant influence on microstructure, particle morphology, and strengthening mechanisms. The strengthening mechanisms of copper alloy coatings include fine crystal reinforcing, solution strengthening, work hardening, and dispersal reinforcing. Different mechanisms are shown to be more or less effective depending on powder composition and the presence of impurities. By filtering impurities before gas atomization, the thermal conductivity of as-sprayed Cu-Cr-Zr coatings can be improved by a factor of two.
Proceedings Papers
ITSC2012, Thermal Spray 2012: Proceedings from the International Thermal Spray Conference, 568-573, May 21–24, 2012,
Abstract
View Paper
PDF
TiAl 3 -Al composite coating on γ-TiAl alloy was prepared by cold spray and subsequent heat-treatment. The Oxidation test, which was carried out at 950 °C in air, indicated that the bare alloy exhibited poor oxidation resistance, significant weight loss was observed after oxidation for 70 h. The oxides formed were the mixture of TiO 2 /Al 2 O 3 . For the specimen with the TiAl 3 –Al coating, great improvement in oxidation resistance was observed. Approximate parabolic oxidation kinetics was observed for the oxidation period. The microstructure analysis showed a dense TiAl 2 interlayer and a reticular Cr rich phase formed between the composite coating and the substrate. The oxides in the oxidized coating were mainly alumina, with only trace of titanium dioxide and titanium nitrides after oxidation up to 1000 h. A certain amount of TiAl 3 phase in the coating remained unoxidized and unconsumed. The EPMA analyses of the coated samples showed that no trend of oxygen or nitride diffusion into the substrate and no oxide formed beneath the TiAl 2 interlayer.
Proceedings Papers
ITSC 2010, Thermal Spray 2010: Proceedings from the International Thermal Spray Conference, 445-449, May 3–5, 2010,
Abstract
View Paper
PDF
Atmospheric plasma spraying (APS) is one of the most promising methods for manufacturing the components employed in solid oxide fuel cells (SOFCs) due to its fast deposition rate and cost-effective characteristics. The anode activity can be improved through increasing the triple-phase boundaries (TPBs) at the electrolyte/anode interface. The active TPBs length, and consequently the performance of the cell, can be enhanced by varying the compositions and microstructure of the APS anode. In this paper, agglomerated powders of NiO and YSZ are prepared by a spray-drying method for preparation of SOFCs anode. The anode was deposited using NiO/YSZ composite powder by APS at different plasma arc power. The influences of plasma arc power on the microstructure and electrochemical performance of Ni/YSZ anode are investigated for the optimization of SOFCs anode.
Proceedings Papers
ITSC 2009, Thermal Spray 2009: Proceedings from the International Thermal Spray Conference, 669-672, May 4–7, 2009,
Abstract
View Paper
PDF
A composite coating using mixed powders of pure Al and α-Al 2 O 3 as feedstock was deposited on AZ91D alloy substrate by cold spraying. The content of α-Al 2 O 3 in mixed powders was 50wt%. Electrochemical experiments were carried out using 3.5wt.% NaCl solution as electrolyte. Because of dense structure, the composite coating could separate substrate from electrolyte thoroughly for long time immersion. The corrosion behavior of the composite coating was evaluated by using electrochemical impedance spectroscopy (EIS) and potentiodynamic polarization measurements. It is found that the composite coating presented much better corrosion resistance than bare AZ91D alloy, even than bulk 1050 aluminum by electrochemical studies in 3.5wt.% NaCl solution.
Proceedings Papers
ITSC 2008, Thermal Spray 2008: Proceedings from the International Thermal Spray Conference, 1406-1410, June 2–4, 2008,
Abstract
View Paper
PDF
During plasma spraying, high substrate temperature contributes to increase the interface temperature between flattening droplet and substrate and subsequently promotes the through-lamella grain growth in the coating. In this study, yttria stabilized zirconia (YSZ) coatings are prepared by atmospheric plasma spray (APS) on the stainless steel substrate preheated to different temperatures from room temperature to 1100°C. The microstructure of the coatings is characterized from polished and fractured cross sections by SEM. The ionic conductivities of the coatings are measured using both DC and AC methods, and the relationship between ionic conductivity and microstructure of coatings is examined. SEM observation shows that the coatings exhibit different microstructures with different substrate temperatures. With the increase of substrate temperature, the columnar grain growth continuously across lamellar interfaces is enhanced and subsequently the intersplat bonding ratio in the coating is increased. The ionic conductivity of YSZ coatings at the direction perpendicular to coating surface is significantly increased through the microstructure development by increasing deposition temperature.
Proceedings Papers
Study on Cold-Sprayed Copper Coating’s Properties and Optimizing Parameters for the Spraying Process
ITSC 2005, Thermal Spray 2005: Proceedings from the International Thermal Spray Conference, 178-184, May 2–4, 2005,
Abstract
View Paper
PDF
Cold gas dynamic spraying is a promising technology and successfully applied to a wide range of materials. In this paper, orthogonal experimental method was introduced to seek out the optimal parameters for cold spraying copper coating. According to the results, standoff distance influenced the coating’s quality the most significantly as well as the carrier gas temperature had a remarkable impact either, but the carrier gas pressure and controlling voltage which influenced feeding speed subsequently had little influence on the coating’s quality. The coating’s porosity, bonding strength, microhardness and the coating’s conductivity were determined respectively. More over, optical and scanning electron microscopies were introduced to study the coating’s surface morphology and its internal structure. Also the effect of subsequent heat treatment on coating’s microhardness was investigated.