Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Subjects
Article Type
Volume Subject Area
Date
Availability
1-1 of 1
S. Schammer
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Proceedings Papers
ITSC1999, Thermal Spray 1999: Proceedings from the United Thermal Spray Conference, 223-227, March 17–19, 1999,
Abstract
View Papertitled, Nachbehandlung thermisch gespritzter Schichten auf Magnesiumwerkstoffen (Post-Treatment of Coatings Plasma-Sprayed Onto Magnesium Alloys)
View
PDF
for content titled, Nachbehandlung thermisch gespritzter Schichten auf Magnesiumwerkstoffen (Post-Treatment of Coatings Plasma-Sprayed Onto Magnesium Alloys)
In this paper results of the alloying of magnesium materials by a combination of thermal spraying and a subsequent electron beam surface technology are presented. The objective is to improve the wear resistance of magnesium alloys. Aluminium and copper were chosen as the alloying material. These metals can form hard intermetallic compounds with magnesium, such as MgAl2 or Mg2Cu. The vacuum plasma spraying is well suited for the deposition of these additives because of the prevention of their oxidation. Besides, the EB technology take place under vacuum conditions, and the reactions between magnesium and oxygen are prevented. Paper text in German.