Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Subjects
Article Type
Volume Subject Area
Date
Availability
1-1 of 1
R. Olsson
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Proceedings Papers
ITSC 2015, Thermal Spray 2015: Proceedings from the International Thermal Spray Conference, 210-216, May 11–14, 2015,
Abstract
View Paper
PDF
Laser-assisted cold-spray has been recognized for over a decade as a technique capable of depositing high quality coatings. By laser heating (and hence softening) the surface being coated, deposition can occur at particle velocities lower than those normally associated with the cold spray process. This can be used to increase deposition rate. However, it can also be used to facilitate the deposition of higher hardness material combinations, normally more out of the reach of the conventional cold spray process. Laser heating can also reduce the requirements of the process on gas usage and gas heating for a given combination, making it more cost-effective. In the work reported below, the capability of a novel co-axially laser-assisted system (COLA) to deposit higher hardness materials, relevant to a range of different industrial applications, has been evaluated. This system can be retrofitted to conventional cold spray equipment.