Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Subjects
Article Type
Volume Subject Area
Date
Availability
1-1 of 1
Qing Jia
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Proceedings Papers
Preparation of Inorganic Phosphate Ceramic Coatings on γ-TiAl Based Alloys
Available to Purchase
ITSC 2015, Thermal Spray 2015: Proceedings from the International Thermal Spray Conference, 150-154, May 11–14, 2015,
Abstract
View Papertitled, Preparation of Inorganic Phosphate Ceramic Coatings on γ-TiAl Based Alloys
View
PDF
for content titled, Preparation of Inorganic Phosphate Ceramic Coatings on γ-TiAl Based Alloys
In this paper, we reported our investigation on preparing inorganic phosphate ceramic coatings on the surface of γ-TiAl based alloy by air spray. The high temperature performance of the coatings was tested by thermal shock test, cyclic oxidation and isothermal oxidation at 950 °C. The results showed that the coatings exhibited significant improvement on high temperature anti-oxidation performance of the base alloy. No obvious cracks or spalling of the coatings occurred after oxidation experiment under isothermal oxidation condition at 950 °C for 1000 h. The characterization was carried out to analyze the microstructure of the coatings before and after oxidation test.