Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Volume Subject Area
Date
Availability
1-10 of 10
P.E. Fischione
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Precise Final Specimen Thinning by Concentrated Argon Ion Beam Milling of Plan View TEM Specimens Prepared in the Xenon Plasma FIB
Available to Purchase
Journal: EDFA Technical Articles
EDFA Technical Articles (2024) 26 (4): 20–26.
Published: 01 November 2024
Abstract
View articletitled, Precise Final Specimen Thinning by Concentrated Argon Ion Beam Milling of Plan View TEM Specimens Prepared in the Xenon Plasma FIB
View
PDF
for article titled, Precise Final Specimen Thinning by Concentrated Argon Ion Beam Milling of Plan View TEM Specimens Prepared in the Xenon Plasma FIB
Xenon plasma focused ion beam specimen preparation is ideal for preparing plan view TEM specimens due to its large-volume-milling capabilities. This article describes concentrated Ar ion beam milling using low energy as a post-pFIB final thinning step of plan view TEM specimens from a phase change memory device. Precise control of specimen thinning is achieved, which results in high-quality specimens with pristine surfaces and a large field of view for TEM characterization.
Proceedings Papers
Enhanced TEM Specimen Preparation for STEM-EBIC Analysis Using a Ga FIB system Followed by Post-FIB Ar Ion Beam Milling
Available to Purchase
ISTFA2024, ISTFA 2024: Conference Proceedings from the 50th International Symposium for Testing and Failure Analysis, 191-199, October 28–November 1, 2024,
Abstract
View Papertitled, Enhanced TEM Specimen Preparation for STEM-EBIC Analysis Using a Ga FIB system Followed by Post-FIB Ar Ion Beam Milling
View
PDF
for content titled, Enhanced TEM Specimen Preparation for STEM-EBIC Analysis Using a Ga FIB system Followed by Post-FIB Ar Ion Beam Milling
Electrical characterization is a critical step in the failure analysis workflow, a sequence that often ends in high-resolution imaging in the transmission electron microscope (TEM). Scanning TEM electron beam-induced current (STEM EBIC) is a technique that effectively combines these methods by performing electrical characterization at each imaging pixel, with the electron beam acting as a local current source. This work highlights the specimen preparation technique using the Ga FIB system followed by post-FIB Ar ion milling for STEM EBIC analysis. We present STEM EBIC as a technique to evaluate the surface quality of the specimens and to characterize the electronic properties of advanced devices at high resolution. With STEM EBIC, inactive and active finFET structures were clearly distinguished and improvements in sample quality from post-FIB Ar ion milling were evident.
Proceedings Papers
Precise Final Thinning by Concentrated Ar Ion Beam Milling of Plan View TEM Specimens from Phase Change Memory Device Prepared in Xe Plasma FIB
Available to Purchase
ISTFA2023, ISTFA 2023: Conference Proceedings from the 49th International Symposium for Testing and Failure Analysis, 309-316, November 12–16, 2023,
Abstract
View Papertitled, Precise Final Thinning by Concentrated Ar Ion Beam Milling of Plan View TEM Specimens from Phase Change Memory Device Prepared in Xe Plasma FIB
View
PDF
for content titled, Precise Final Thinning by Concentrated Ar Ion Beam Milling of Plan View TEM Specimens from Phase Change Memory Device Prepared in Xe Plasma FIB
Advanced memory technologies are in demand with phase change memory (PCM) devices as a forefront candidate. For successful characterization by transmission electron microscopy (TEM) for failure analysis and device development, an accurate and controllable thinning of TEM specimens is critical. In this work, TEM specimens from a GeTe-based PCM device at a partial SET state were prepared using a Xe plasma focused ion beam (pFIB) and polished to electron transparency using Ar ion beam milling. We will highlight the differences between Ga focused ion beam (FIB) and Xe pFIB TEM specimen preparation, the benefits of post-pFIB Ar ion beam milling, and show TEM results of the effects of partial SET programming of the GeTe PCM device.
Proceedings Papers
Large Field of View and Artifact-Free Plan View TEM Specimen Preparation by Post-FIB Ar Milling
Available to Purchase
ISTFA2022, ISTFA 2022: Conference Proceedings from the 48th International Symposium for Testing and Failure Analysis, 181-189, October 30–November 3, 2022,
Abstract
View Papertitled, Large Field of View and Artifact-Free Plan View TEM Specimen Preparation by Post-FIB Ar Milling
View
PDF
for content titled, Large Field of View and Artifact-Free Plan View TEM Specimen Preparation by Post-FIB Ar Milling
Semiconductor devices are decreasing in dimensions and currently comprise stacks of ultrathin layers as in a spin-transfer torque magnetoresistive random-access memory (STTMRAM) device. For successful characterization by transmission electron microscopy (TEM) for failure analysis and device development, an accurate and controllable thinning of TEM specimens for is desirable. In this work, we combine plan view Ga focused ion beam (FIB) and post-FIB Ar milling preparation to prepare TEM specimens from a STT-MRAM device. Post-FIB Ar milling technique as a final polishing step of plan view TEM specimens was shown to prevent exposure of the tunnel barrier layer that can be damaged by the Ga FIB beam. We discuss the plan view FIB preparation, post-FIB Ar milling step and image analysis of the TEM images.
Proceedings Papers
Accurate Sub-micron Device Delayering of Plan View TEM Specimens By Ar Ion Milling
Available to Purchase
ISTFA2021, ISTFA 2021: Conference Proceedings from the 47th International Symposium for Testing and Failure Analysis, 135-140, October 31–November 4, 2021,
Abstract
View Papertitled, Accurate Sub-micron Device Delayering of Plan View TEM Specimens By Ar Ion Milling
View
PDF
for content titled, Accurate Sub-micron Device Delayering of Plan View TEM Specimens By Ar Ion Milling
This paper describes an accurate and controllable delayering process to target defects in new materials and device structures. The workflow is a three-step process consisting of bulk device delayering by broad Ar ion beam milling, followed by plan view specimen preparation using a focused ion beam, then site-specific delayering via concentrated Ar ion beam milling. The end result is a precisely delayered device without sample preparation-induced artifacts suitable for identifying defects during physical failure analysis.
Proceedings Papers
Cutting-Edge Sample Preparation from FIB to Ar Concentrated Ion Beam Milling of Advanced Semiconductor Devices
Available to Purchase
ISTFA2020, ISTFA 2020: Papers Accepted for the Planned 46th International Symposium for Testing and Failure Analysis, 133-140, November 15–19, 2020,
Abstract
View Papertitled, Cutting-Edge Sample Preparation from FIB to Ar Concentrated Ion Beam Milling of Advanced Semiconductor Devices
View
PDF
for content titled, Cutting-Edge Sample Preparation from FIB to Ar Concentrated Ion Beam Milling of Advanced Semiconductor Devices
Fast and accurate examination from the bulk to the specific area of the defect in advanced semiconductor devices is critical in failure analysis. This work presents the use of Ar ion milling methods in combination with Ga focused ion beam (FIB) milling as a cutting-edge sample preparation technique from the bulk to specific areas by FIB lift-out without sample-preparation-induced artifacts. The result is an accurately delayered sample from which electron-transparent TEM specimens of less than 15 nm are obtained.
Proceedings Papers
Low Energy Ar Ion Milling of FIB TEM Specimens from 14 nm and Future FinFET Technologies
Available to Purchase
ISTFA2018, ISTFA 2018: Conference Proceedings from the 44th International Symposium for Testing and Failure Analysis, 241-246, October 28–November 1, 2018,
Abstract
View Papertitled, Low Energy Ar Ion Milling of FIB TEM Specimens from 14 nm and Future FinFET Technologies
View
PDF
for content titled, Low Energy Ar Ion Milling of FIB TEM Specimens from 14 nm and Future FinFET Technologies
Transmission electron microscopy (TEM) specimens are typically prepared using the focused ion beam (FIB) due to its site specificity, and fast and accurate thinning capabilities. However, TEM and high-resolution TEM (HRTEM) analysis may be limited due to the resulting FIB-induced artifacts. This work identifies FIB artifacts and presents the use of argon ion milling for the removal of FIB-induced damage for reproducible TEM specimen preparation of current and future fin field effect transistor (FinFET) technologies. Subsequently, high-quality and electron-transparent TEM specimens of less than 20 nm are obtained.
Proceedings Papers
Ion Milling of Ex-Situ Lift-Out FIB Specimens
Available to Purchase
ISTFA2017, ISTFA 2017: Conference Proceedings from the 43rd International Symposium for Testing and Failure Analysis, 260-264, November 5–9, 2017,
Abstract
View Papertitled, Ion Milling of Ex-Situ Lift-Out FIB Specimens
View
PDF
for content titled, Ion Milling of Ex-Situ Lift-Out FIB Specimens
The semiconductor industry is constantly investigating new methods that can improve both the quality of TEM lamella and the speed at which they can be created. To improve throughput, a combination of FIB-based preparation and ex situ lift-out (EXLO) techniques have been used. Unfortunately, the carbon support on the EXLO grid presents problems if the lamella needs to be thinned once it is on the grid. In this paper, we present low-energy (<1 keV), narrow-beam (<1 μm diameter), Ar+ ion milling as a method of preparing electron-transparent and gallium-free EXLO FIB specimens.
Proceedings Papers
Automated End-Point Detection and Targeted Ar + Milling of Advanced Integrated Circuit FIB TEM Specimens
Available to Purchase
ISTFA2017, ISTFA 2017: Conference Proceedings from the 43rd International Symposium for Testing and Failure Analysis, 375-379, November 5–9, 2017,
Abstract
View Papertitled, Automated End-Point Detection and Targeted Ar + Milling of Advanced Integrated Circuit FIB TEM Specimens
View
PDF
for content titled, Automated End-Point Detection and Targeted Ar + Milling of Advanced Integrated Circuit FIB TEM Specimens
The sub-nanometer resolution that transmission electron microscopy (TEM) provides is critical to the development and fabrication of advanced integrated circuits. TEM specimens are usually prepared using the focused ion beam, which can cause gallium-induced artifacts and amorphization. This work presents the use of a concentrated argon ion beam for reproducible TEM specimen preparation using automatic milling termination and targeted ion milling of device features; the result is high-quality and electron-transparent specimens of less than 30 nm. Such work is relevant for semiconductor product development and failure analysis.
Proceedings Papers
Advanced Tools and Techniques for Delayering and Cross-Sectioning Semiconductor Devices
Available to Purchase
ISTFA2017, ISTFA 2017: Conference Proceedings from the 43rd International Symposium for Testing and Failure Analysis, 592-596, November 5–9, 2017,
Abstract
View Papertitled, Advanced Tools and Techniques for Delayering and Cross-Sectioning Semiconductor Devices
View
PDF
for content titled, Advanced Tools and Techniques for Delayering and Cross-Sectioning Semiconductor Devices
Conventional mechanical sample preparation is a difficult and uncontrolled process that does not allow targeting of a specific depth or layer. Because of the difficulties presented by mechanical sample preparation, there has been an emergence of beam-based techniques for device delayering applications. Cross-sectioning is another commonly used technique used in microelectronics industry investigations; when combined with delayering, one can gain complete knowledge about a device's faults. This paper presents a development in semiconductor device investigation using low energy, broad-beam argon ion milling. The results highlight that broad-beam Ar ion milling produces excellent surface quality, which allows high resolution scanning electron microscope observation and energy dispersive spectrometry analyses, even at low energy.