Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Article Type
Volume Subject Area
Date
Availability
1-1 of 1
P. Peetsalu
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Proceedings Papers
Thermal Spray Coatings from WC-Co Powders Produced by Mechanically Activated Synthesis
Available to Purchase
ITSC 2006, Thermal Spray 2006: Proceedings from the International Thermal Spray Conference, 1387-1392, May 15–18, 2006,
Abstract
View Papertitled, Thermal Spray Coatings from WC-Co Powders Produced by Mechanically Activated Synthesis
View
PDF
for content titled, Thermal Spray Coatings from WC-Co Powders Produced by Mechanically Activated Synthesis
In the present study WC-Co feedstock powder was produced by the process termed mechanically activated synthesis (MAS). The main characteristics of the powder (particle/granules size, size distribution, morphology, chemical composition and granules microstructure) were determined. The material was sprayed by the HVOF process to investigate the properties of the coatings in comparison to standard materials. The microstructure, phase structure, porosity and microhardness values of the coatings were studied. The abrasion wear resistance of the coatings was evaluated by rubber wheel abrasion tests. Results of abrasive wear tests show that the new material has superior properties compared to conventional WC-Co coatings.