Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Article Type
Volume Subject Area
Date
Availability
1-1 of 1
M. S. Liang
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Proceedings Papers
ISTFA2005, ISTFA 2005: Conference Proceedings from the 31st International Symposium for Testing and Failure Analysis, 413-415, November 6–10, 2005,
Abstract
View Papertitled, Effect of Ash Chemistries on TDDB Lifetime of Cu/ULK Interconnects
View
PDF
for content titled, Effect of Ash Chemistries on TDDB Lifetime of Cu/ULK Interconnects
The effect of ash chemistries, N2/H2 and H2, on time-dependent dielectric breakdown (TDDB) lifetime has been investigated for Cu damascene structure with a carbon-doped CVD ultra low-k (ULK, k=2.5) intermetal dielectric. Two failure modes, interfacial Cu-ion-migration and Cu diffusion through the bulk intermetal ULK were attributed to the TDDB degradation for the H2 ash.The interfacial Cu-ion-migration was the only dominated failure mode for the N2/H2 ash. The nitrogen species in the N2/H2 plasma proved to be capable of forming a nitrided protection layer on the surface of the ULK. This nitrided layer suppressed further plasma damage during the ash process and thus lessened the TDDB degradation by preventing Cu diffusion through the bulk ULK.