Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Subjects
Article Type
Volume Subject Area
Date
Availability
1-1 of 1
Linhua Zhang
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Proceedings Papers
ISTFA2022, ISTFA 2022: Conference Proceedings from the 48th International Symposium for Testing and Failure Analysis, 365-368, October 30–November 3, 2022,
Abstract
View Paper
PDF
In wafer fabrication, silicon defects on the substrate directly affect the yield of the wafer. In this paper, we will study and discuss a chemical delayering and delineate method for silicon defects in wafer fabrication using Secco etch. It is well-known that during delayering process of wafer, the removal of polysilicon (Poly-Si) layer is very difficult, especially for the wide-layer polysilicon (Poly-Si) which is difficult to completely remove with HF acid solution. We introduce a chemical recipe to fast delayer polysilicon layer completely before delineating silicon defects on silicon substrate using Secco etch. Those skilled in the art could be experiment within half an hour to get analysis results. It saves time and improves operational efficiency. Moreover, based on the experimental results we think that it is possible to identify the root cause according to the shapes of silicon defects using Secco etch.