Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Article Type
Volume Subject Area
Date
Availability
1-1 of 1
K. Schlimbach
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Proceedings Papers
ITSC1999, Thermal Spray 1999: Proceedings from the United Thermal Spray Conference, 410-413, March 17–19, 1999,
Abstract
View Papertitled, Möglichkeiten zur Verbesserung der Verschleißeigenschaften von Aluminium-Legierungen durch Plasma-Pulver-Schweißverfahren (Possibilities for Improving Wear-Properties of Aluminium-Alloys by Plasma Powder Welding Process)
View
PDF
for content titled, Möglichkeiten zur Verbesserung der Verschleißeigenschaften von Aluminium-Legierungen durch Plasma-Pulver-Schweißverfahren (Possibilities for Improving Wear-Properties of Aluminium-Alloys by Plasma Powder Welding Process)
Aluminium alloys are extensively used materials which can be found in all kinds of industrial applications. They have distinctive advantages such as a high strength/weight ratio, an excellent workability and a good corrosion behaviour. However, aluminium alloys have wear resistance properties which limitate further use of these alloys. Plasma transferred arc surfacing (PTA) using the DCCP-technology (Direct Current Combined Polarity) was used for enhancing wear properties of different aluminium alloys (AlMgSi0.5, AlSi12) by the formation of an alloyed layer with added ceramics. Hardness of the base material could be increased by more than two times while the wear resistance of the modified aluminium alloy was about ten times higher compared to the base material. Paper text in German.