Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Article Type
Volume Subject Area
Date
Availability
1-1 of 1
Jan Valdman
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Proceedings Papers
SMST2024, SMST 2024: Extended Abstracts from the International Conference on Shape Memory and Superelastic Technologies, 82-83, May 6–10, 2024,
Abstract
View Papertitled, Constitutive Model for NiTi Polycrystalline Alloys Undergoing Transformation and Plastic Deformation Processes
View
PDF
for content titled, Constitutive Model for NiTi Polycrystalline Alloys Undergoing Transformation and Plastic Deformation Processes
Great attention has been recently paid to the investigation of plastic deformation in NiTi. Experimental investigations of the mechanical response of NiTi polycrystalline samples within a broad stress-strain-temperature state space have revealed a complex response involving martensitic transformation, reorientation, and plastic deformation processes. The interactions between them result in complex coupled phenomena, such as transformation-induced plasticity, martensite stabilization through plastic deformation, and micro-strain heterogeneity induced by plasticity. Plastic deformation in NiTi not only generates irrecoverable strain at the macroscale, but it also induces substantial strain heterogeneity in the microstructure. This heterogeneity significantly affects the functional properties and may open up new technology pathways for designing sophisticated products. Tailored constitutive models that can reproduce the response in complex loading scenarios can be extremely beneficial.