Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Subjects
Article Type
Volume Subject Area
Date
Availability
1-1 of 1
Jan Michalička
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Proceedings Papers
ISTFA2015, ISTFA 2015: Conference Proceedings from the 41st International Symposium for Testing and Failure Analysis, 65-70, November 1–5, 2015,
Abstract
View Paper
PDF
Reducing FIB induced damage on TEM samples is very important in order to preserve the sample structure, especially on modern semiconductor devices. We have compared the damage caused by Ga ion beam to our measurements of the damage caused by Xe ion beam and came to the conclusion that Xe ion beam induced damage is significantly lower at 30 keV beam energy. This has been proven by several independent analytical methods. Our results show that TEM sample preparation by Xe ion beam causes less amorphous damage and increase the quality of the lamella and in many cases it will allow to prepare the lamella by finishing it even at 30 keV, without the final cleaning step at the low beam energy. Final polishing step by Xe beam at beam energy 3 keV further reduces the amorphous layer, but the difference against Ga beam is not so significant like at 30 keV.