Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Article Type
Volume Subject Area
Date
Availability
1-1 of 1
Jan A. Frenzel
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Proceedings Papers
SMST2024, SMST 2024: Extended Abstracts from the International Conference on Shape Memory and Superelastic Technologies, 117-118, May 6–10, 2024,
Abstract
View Papertitled, Processing and Thermomechanical Stability of Low Hysteresis Shape Memory Alloys
View
PDF
for content titled, Processing and Thermomechanical Stability of Low Hysteresis Shape Memory Alloys
NiTi shape memory alloy (SMA) actuators have gained much attention in recent years because of their ability to combine high actuation forces to a significantly smaller component size. Binary SMAs containing Ni and Ti, however, suffer from relatively poor functional and structural fatigue, which requires training. Binary NiTi SMAs also possess a relatively wide hysteresis gap between the austenite final and martensite final temperatures (ΔT MfAf ), which demands more energy to produce each actuation stroke. Zarnetta et al. have shown that small additions of substitutional elements to the NiTi-based SMA can significantly improve those conditions by increasing the coherency between the two transforming crystal structures. Two quaternary NiTiCuPd SMAs were selected based on combinatorial studies from X-ray diffraction data and their results were analyzed concerning their hysteresis width and thermal-mechanical stability.