Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Article Type
Volume Subject Area
Date
Availability
1-2 of 2
J. Bensch
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Proceedings Papers
ITSC 2009, Thermal Spray 2009: Proceedings from the International Thermal Spray Conference, 361-365, May 4–7, 2009,
Abstract
View Paper
PDF
This work investigates the influence of plasma-sprayed deposits on the fatigue life of coated specimens. Hydroxyapatite (HA) and TiO 2 were deposited on dog-bone shaped substrates under different spraying conditions while measuring in-flight particle temperature and velocity. The coated specimens were then subjected to cyclic bending with constant deflection and the number of cycles to failure was recorded. It was found that the higher the temperature and velocity of particles during spraying, the greater the improvement in fatigue life up to a maximum of 46% compared to uncoated samples.
Proceedings Papers
ITSC 2007, Thermal Spray 2007: Proceedings from the International Thermal Spray Conference, 727-732, May 14–16, 2007,
Abstract
View Paper
PDF
To prepare a dense, defect-free deposit of refractory metals relies not only on the droplets’ state, their temperature and velocity prior to impact on the surface of substrate and/or the precedent deposited layer, but also on the surface temperature of the substrate, whereupon the droplets impact. This paper presents a comprehensive investigation, in which the particles temperature, velocity, and the substrate temperature are studied all-in-one step to understand their influence on the deposit quality. The experimental results make our knowledge of the induction plasma spray of refractory metals process more integrated. Based on our estimation on the effect of all of the three factors, a set of optimized process parameters was established and proved by applying it in producing stationary deposits and coating layers. The results obtained distinguish the induction plasma spray a unique technique, which is ideal to be utilized in refractory metals deposit.