Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Article Type
Volume Subject Area
Date
Availability
1-1 of 1
H. Tai
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Proceedings Papers
Alumina Coatings by Plasma Spraying of Monosize Sapphire Particles
Available to Purchase
ITSC1998, Thermal Spray 1998: Proceedings from the International Thermal Spray Conference, 791-796, May 25–29, 1998,
Abstract
View Papertitled, Alumina Coatings by Plasma Spraying of Monosize Sapphire Particles
View
PDF
for content titled, Alumina Coatings by Plasma Spraying of Monosize Sapphire Particles
In an effort to obtain a series of plasma-sprayed coatings of controlled microstructure, three monosized sapphire powders were deposited using an axial injection torch in which the plasma gas composition and nozzle diameter were the only parameters varied. The effect of these parameters on splat morphology, porosity, angular crack distribution, and hardness is reported. Uniform, dense microstructure with a hardness rivaling chromia coatings was achieved through a combination of tightly controlled processing conditions and the use of mono-disperse precursor powders.