Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Article Type
Volume Subject Area
Date
Availability
1-1 of 1
G. Sitte
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Proceedings Papers
ITSC1999, Thermal Spray 1999: Proceedings from the United Thermal Spray Conference, 414-417, March 17–19, 1999,
Abstract
View Papertitled, Rollennaht-Auftragschweißen – eine Alternative zum thermischen Spritzen hochbeanspruchter Oberflächen (Resistance Roller Seam Deposition Welding – An Alternative for Thermal Spraying of High Strained Surfaces)
View
PDF
for content titled, Rollennaht-Auftragschweißen – eine Alternative zum thermischen Spritzen hochbeanspruchter Oberflächen (Resistance Roller Seam Deposition Welding – An Alternative for Thermal Spraying of High Strained Surfaces)
Resistance seam surfacing is an economic alternative for thermal spraying especially for high abrasion wear on surfaces of simple geometry. First tests have shown that this process can also be used for producing wear protection layers on aluminium surfaces. The advantages of this process are very low energy costs, no danger for health, no loss of powder, a relatively low process temperature and a good quality of the layer. Paper text in German.